The appearance of freeze-dried products is good in uniform color, dense pores, maintaining the volume and properties before freeze-drying, and forming a spongy block structure.
Sometimes the product looks good before it comes out of the box, and then there are voids and pieces soon after it comes out of the box.
The main reason is that the product is not completely dried, and there are still ice crystals. After the product is out of the box, the temperature and pressure of the product are above the eutectic point.
The ice melts into water, and the water is absorbed by the surrounding dried matter, resulting in void shrinkage. Incomplete drying means that the drying time is not long enough or the temperature is too low, or both;
otherwise, the freezing rate is too fast, the grains are too fine, and the sublimation rate is slowed down; or the freezing is not complete; or the finished product is not sealed after freeze-drying. In order to absorb the moisture in the air and shrink, the nitrogen filling method can be used.
When the product is out of the box, it has a skeleton structure with a large gap, or even a fluff-like structure. After the product is out of the box, the fluff-like structure material quickly dissipates.
The reason is that the product formula contains less solid matter, and free water freezes into ice when it freezes, occupying a large volume, and the voids formed after sublimation are also large.
The useful components are dispersed with water vapor during sublimation, forming plush. It will absorb water vapor and disappear when it encounters air. It should be solved by adding an appropriate amount of filler.
When the product is out of the box, defects such as bubble pits, dry shrinkage, collapse, and voids appear.
The reason is that the freezing temperature is too high, or the time is too short, and the product is completely frozen; or the temperature in the drying stage is too high, and the pressure is too high.
Caused by melting some products.
Vacuum sublimation is performed before it is frozen, and the external pressure decreases rapidly to cause bubbling; the melted product produces vapor concentration and shrinks; some wet products are heated and melted violently, which will melt the dried object and form a cavity to collapse.
Therefore, it must be frozen, and the sublimation cannot exceed the eutectic temperature and disintegration temperature of the product.
The color and pores of the product are uneven in the depth direction. Due to the long storage time after packaging, some substances in the solution are precipitated or the insoluble components are precipitated.

The influencing factors of product appearance also include solution concentration and outgassing speed. The concentration of the solution is generally controlled between 10~15%, and excipients should be added if the concentration is less than 5%.
If the concentration is too high, the thickness should be controlled, generally 10~15mm. If the solution concentration is greater than 30%, the product is prone to shrinkage, collapse and incompleteness.
In addition, the frozen surface is first dehydrated during drying to form a dry shell with a dense structure, and the sublimated water vapor below escapes from the gaps between the molecules of the dried surface.
At this time, if the concentration of the solution is too high, the gap between molecules is small, the ventilation is poor, the resistance of water vapor passing through is large, and a large number of water molecules cannot escape in time,
and the stagnation time in the drying layer is long, so that some of the dried drugs are gradually deliquescent, which will cause The volume of the product shrinks, and the shape is not full or collapsed.
If the weight concentration of the liquid medicine is less than 4%, the medicine will be scattered with the water vapor when the vacuum is applied; or it will become a fluff-like loose structure after drying. into a hollow shape. Another situation is that the concentration of the liquid medicine is too low, which makes the product loose and easy to attract moisture.
At the same time, because the specific surface area is too large, the product is easy to shrink, and the mechanical strength of the dried product is too low. Once vibrated, it will disperse into powder and adhere to the bottle wall. .
In the freeze-drying process, if the thickness of the liquid medicine is greater than 20mm, the drying time will be prolonged, and the appearance of the product will also be unqualified.
In addition, the cooling speed is fast at the beginning of freezing, so that the product forms fine crystals, the density is large, the sublimation resistance is large, the water is not easy to evaporate, the product will gradually deliquesce, resulting in volume shrinkage,
resulting in an incomplete shape or a lump. If the freezing speed is too slow and the ice crystals grow for a long time, concentration is likely to occur, resulting in the separation of the drug and the solvent and the uneven structure of the finished product.
Measures: Rationally design the formulation of the lyophilized solution. Generally, the weight concentration should be between 4% and 25%, and the concentration should be between 10% and 15%.
If the concentration is lower than 4%, excipients (such as mannitol, dextran, lactose, etc.) can be added appropriately. If the concentration is high, the thickness of the freeze-dried product must be controlled, or the concentration must be reduced, and a large container should be used to fill the liquid medicine.
During the freeze-drying process, the cooling rate should be controlled to decrease by 5°C to 6°C per hour. In the first stage of sublimation and drying, the temperature of the product should be lower than the eutectic point, the temperature should not be fast, and it should be controlled at about 5 °C per hour.
If the heating is too fast, when the product has a lot of water, the temperature exceeds its eutectic point, which will cause the product to melt and appear defective.
In the second-stage sublimation stage, although the water content in the product is low at this time, the heating rate can be appropriately increased, but the temperature should be controlled below the safe temperature, otherwise there will be agglomeration.
In addition, the air tightness of the product packaging is not good, and the appearance or even the internal quality will be unqualified within the validity period.
Application of Freeze Dryer